EnduraMet 2205

UNS #S31803

EnduraMet 2205 stainless is a duplex stainless steel that has a microstructure consisting of austenite and ferrite phases. The duplex microstructure and the chemical composition result in an excellent combination of strength and corrosion resistance. EnduraMet 2205 has twice the annealed yield strength of typical austenitic stainless steels, like 304 and 316. In the hot rolled unannealed condition, yield strength of 75 ksi (518 MPa) or higher can be achieved for bar diameters up to 1.375 in. (34.925mm). It possesses good resistance to general corrosion in many acid environments and, has excellent resistance to chloride stress corrosion cracking, pitting and crevice corrosion.

Type Analysis

  • Carbon (Nominal) 0.03
  • Phosphorus (Maximum) 0.03
  • Silicon (Maximum) 1
  • Nickel (Nominal) 5.5
  • Manganese (Maximum) 2
  • Sulfur (Maximum) 0.02
  • Chromium (Nominal) 22
  • Molybdenum (Nominal) 3
  • Iron (Nominal) Balance
  • Nitrogen (Nominal) 0.2

Applications

Rebar including bridge decks, barrier and retaining walls, anchoring systems, chemical plant infrastructure, coastal piers and wharves, bridge parapets, sidewalks and bridge piling, bridge tie wire and dowels; oil and gas production equipment, such as valves, fittings, shafts, and pump parts; heat exchangers in chemical and pulp and paper plants; and brewery tanks

Applicable Specifications

  • ASME SA479
  • ASTM A276
  • ASTM A955M
  • NACE MR0175
  • ASTM A240
  • ASTM A479
  • BS 6744: 2001

Bar

Billet

Rebar-Bar-Reinforcing

Rod

Rounds

Strip

Wire