UNS #S41429

A-21® is an advanced martensitic stainless steel that offers a unique combination of high strength, excellent toughness, and outstanding stainless properties in the carburized, nitrided, and quenched & tempered conditions. It is available as VIM-VAR, VAR, or air melt. In the carburized condition, A-21® is the world’s first and only truly stainless carburizing steel, developing a deep, hard, stainless case and a strong, tough, ductile core.

Type Analysis

  • Carbon (Maximum) 0.13
  • Phosphorus (Maximum) 0.03
  • Silicon (Maximum) 1.0
  • Nickel (Nominal) 2.00-3.00
  • Titanium (Nominal) 0.15-0.75
  • Manganese (Maximum) 0.75
  • Sulfur (Maximum) 0.03
  • Chromium (Nominal) 10.50-14.00
  • Molybdenum (Nominal) 0.40-0.80
  • Iron (Nominal) Balance
  • Aluminum (Maximum) 0.05
  • Copper (Maximum) 0.50
  • Boron (Maximum) 0.01
  • Tin (Maximum)0.02
  • Vanadium (Maximum) 0.25
  • Cobalt (Maximum) 1.0
  • Columbium/Niobium (Maximum)0.20

Downloads

Request a Quote

Applicable Specifications

  • CTC A-21

Bar

Flats

Hollow Bar

Rectangles

Rounds

Square

Billet

Plate

Strip

Coil

Sheet

Wire

Rod

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.