Composition (Nominal)
0.06 C, 1.00 Mn, 0.030 P, 0.030 S, 0.50 Si, 22.00/26.00 Cr, 33.00/37.00 Ni, 5.00/6.70 Mo, 1.00/3.00 Cu, 0.17/0.40 N, Bal. Fe

A 6% Mo austenitic stainless metal alloy possessing a unique combination of corrosion resistance and ultra high tensile strength capability (up to 280 ksi [1930 MPa]) with good ductility. 20Mo-6 HS stainless is the result of compositional and processing modifications made to 20Mo-6 stainless for enhanced work hardening response.