305 Stainless

UNS S30500
Composition (Nominal)
0.12 C, 2.00 Mn, 0.045 P, 0.03 S, 1.00 Si, 17.00/19.00 Cr, 10.50/13.00 Ni, Bal. Fe

Chromium-nickel austenitic stainless steel which has been used extensively for cold heading, severe deep drawing and spinning operations. High nickel content slows work hardening. Maintains low magnetic permeability after cold working.

Specifications: AMS 5685, ASTM A193, ASTM A314, ASTM A320, ASTM A473, ASTM A580