350 Alloy

UNS S35000
Composition (Nominal)
0.07/0.11 C, 0.50/1.25 Mn, 0.04 P, 0.03 S, 0.50 Si, 6.00/17.00 Cr, 4.00/5.00 Ni, 2.50/3.25 Mo, 0.07/0.13 N, Bal. Fe

Chromium-nickel-molybdenum stainless alloy hardenable by martensitic transformation and precipitation hardening. Offers superior corrosion resistance to other quench-hardenable martensitic stainless steels. Good high temperature strength.

Specifications: AMS 5548 (Strip), AMS 5745 (Bar)