41 Alloy

UNS N07041 | AISI 683

Composition (Nominal)
0.06/0.12 C, 0.50 Mn, 0.50 Si, 18.00/20.00 Cr, 9.00/10.50 Mo, 10.00/12.00 Co, 3.00/3.30 Ti, 1.40/1.60 Al, 0.003/0.010 B, 5.00 Fe, Bal. Ni

A nickel-base, precipitation-hardening alloy that exhibits high strength in the 1200/1800°F (649/982°C) temperature range. Has been used in jet engine and high-speed airframe components.

Specifications: AMS 5712, AMS 5713, AMS 5800 (weld rod - chem only) 