410 Stainless

UNS S41000
Composition (Nominal)
0.15 C, 1.00 Mn, 0.040 P, 0.030 S, 1.00 Si, 11.50/13.00 Cr, Bal. Fe

Hardenable martensitic stainless alloy used for highly stressed parts needing good corrosion resistance and strength. Can be heat-treated to obtain high-strength properties with good ductility.

Specifications: AMS 5613, ASTM A276, ASTM A479, ASTM A493, ASTM A580, ASTM F899, QQ-S-763