420F Stainless

UNS S42020
Composition (Nominal)
0.15 C min., 1.25 Mn, 0.06 P, 0.15 S min., 1.00 Si, 12.00/14.00Cr, 0.60 Mo, Bal. Fe

Type 420F, a free-machining version of Type 420, is a hardenable 12% chrome steel with higher strength, hardness, and wear resistance than Type 410.

Specifications: ASTM A582, AMS 5620, QQ-S-764