636 Alloy

UNS S42200 | AISI 6116
Composition (Nominal)
0.20/0.25 C, 1.00 Mn, 1.00 Si, 0.04 P, 0.03 S, 11.50/13.50 Cr, 0.50/1.00 Ni, 0.75/1.25 Mo, 0.75/1.25 W, 0.20/0.50 V, Bal. Fe

Hardenable stainless designed for service to 1200°F (649°C). Good resistance to scaling and oxidation in continuous service at temperatures to 1400°F (760°C). Has been used for compressor and steam turbine buckets and blades.