Single figures are nominal except where noted.
Carbon (Maximum) 0.03 %, Manganese (Maximum) 2.00 %, Phosphorus (Maximum) 0.035 %, Sulfur (Maximum) 0.010 %, Silicon (Maximum) 0.60 %, Chromium 26.00 to 29.00 %, Nickel 3.50 to 5.20 %, Molybdenum 1.00 to 2.50 %, Nitrogen 0.15 to 0.35 %, Iron Balance

7-Mo PLUS stainless is a duplex (two-phase) alloy with about 45% austenite distributed within a ferrite matrix. 7-Mo PLUS stainless possesses good resistance to chloride-stress-corrosion cracking, pitting corrosion, and general corrosion in many severe environments.

Specifications: ASTM A240, ASTM A479, ASTM A789, ASTM A790
7-Mo PLUS stainless can be supplied according to the following ASTM specifications (and their corresponding ASME specifications, as available). This alloy is included in the ASME Boiler and Pressure Vessel Code, Section VIII, Division I, Case Code 2035. Consult CarTech Technology, Trent Tube or authorized distributor for verification of material certification to your specification requirements.

Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »