BioDur® 316LS Stainless

UNS S31673
Composition (Nominal)
0.030 C, 2.00 Mn, 0.75 Si, 0.025 P, 0.010 S, 17.00/19.00 Cr*, 13.00/15.00 Ni, 2.25/3.50 Mo*, 0.50 Cu, 0.10 N, Bal. Fe, (*3.3 x Mo + Cr 26.00)

A vacuum arc remelted, low carbon, high nickel and molybdenum version of Type 316 which has been used in surgical implant devices. The chemistry modifications are designed to maximize the corrosion resistance of this alloy and provide a ferrite free microstructure. Meets the requirements of ASTM F138 Grade 2, ASTM F139 Grade 2 and ISO 5832-1 Composition D.

Specifications: ASTM F138, ASTM F139, ISO 5832-1 Composition D