CTS® 20 Alloy

UNS S42000

Composition (Nominal):
0.33 C, 0.40 Mn, 0.50 Si, 13.50 Cr, Bal. Fe

Has been used for long-run molding jobs and provided good protection against corrosive hazards due to machine shutdowns and storage between runs, plastic compounds, and humid climates.

This alloy is in the CTS™ family of alloys, offering superior edge retention and surface finish, an ability to be machined to a fine edge, and consistent heat-treatability from lot to lot. Consider CTS alloys for many blade applications including commercial food processing, paper processing, textile, packaging, recycling/refuse, kitchen knives, hand tools, scissors/shears, shaving razors, sport/hunting knives, ice skates, military/defense, law enforcement, salon blades and various surgical/medical applications.

PRODUCT RESOURCES

LITERATURE

Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »