CTS® 20CP Alloy

Composition (Nominal)
2.25 C, 0.50 Mn (maximum), 0.030 S, 0.90 Si, 12.80 Cr, 1.30 Mo, 9.25 V, Bal. Fe

A corrosion-resistant, high vanadium wear-resistant tool steel produced using Carpenter's Micro-Melt powder process. The wear resistance of this grade is comparable to Micro-Melt A11-LVC alloy. This alloy is now available in strip product form.