CTS® B52 Alloy

Composition (Nominal):
1.00 C, 0.30 Mn, 0.25 Si, 1.40 Cr, Bal. Fe

A high-carbon, high-chromium-bearing alloy steel possessing deep hardening characteristics as well as high wear resistance. This alloy is now available in Strip product form.

CTS B52 is a member of Carpenter's CTS™ family of alloys that offer superior edge retention and surface finish, along with an ability to be machined to a fine edge and consistent heat-treatability from lot to lot. Consider CTS alloys for a wide array of blade applications, including commercial food processing, paper processing, textile, packaging, recycling/refuse, kitchen knives, cutting tools, scissors/shears, shaving razors, sport/hunting knives, ice skates, military/defense, law enforcement, salon blades and various surgical/medical applications.

Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »