Greek Ascoloy Alloy

UNS S41800
Composition (Nominal)
0.15/0.20 C, 0.50 Mn, 0.50 Si, 0.03 P, 0.03 S, 12.00/14.00 Cr, 1.80/2.20 Ni, 0.50 Mo, 2.50/3.50 W, Bal. Fe

This martensitic alloy is designed for service at temperatures to 1200°F (649°C) in highly stressed parts. Extremely deep hardening.

Specifications: AMS 5616, ASME 615