H-46 Alloy

Single figures are nominal except where noted.
Carbon 0.15 to 0.20 %, Manganese 0.50 to 0.80 %, Silicon 0.20 to 0.60 %, Chromium 10.00 to 14.00 %, Nickel 0.30 to 0.60 %, Molybdenum 0.50 to 1.00 %,
Columbium + Tantalum 0.20 to 0.60 %, Vanadium 0.20 to 0.40 %, Nitrogen 0.04 to 0.10 %, Iron Balance

Carpenter H-46 is a martensitic, 12% chromium steel designed primarily for high strength applications in the 900/1200°F (482/649°C) temperature range.

The creep resisting properties of this alloy compare favorably with those of several of the lower grades of austenitic, heat resisting steels in the 1000/1200°F (538/649°C) temperature range.

H-46 exhibits low thermal expansion properties. This has been a factor for its consideration for use in structural applications where standard austenitic stainless steels have been inadequate due to excessive expansion when heated.

Applications

H-46 has been used in compressor blades and rotor discs in jet aircraft engines, as well as in other applications requiring high strength in the 900/1200°F (482/649°C) temperature range.