Hipernom® Alloy


Single figures are nominal except where noted.
Carbon 0.02 %, Manganese 0.50 %, Silicon 0.35 %, Nickel 80.00 %, Molybdenum 4.20 %, Iron Balance

Hipernom® alloy is a soft magnetic alloy containing approximately 80% nickel, 4.20% molybdenum, and 15% iron which develops extremely high permeabilities with minimum hysteresis loss. Its analysis is the same as that of Carpenter HyMu "80"® alloy, which is available in strip, bar, wire and billet form.

Hipernom alloy has been used primarily in shielding applications to protect electrical equipment from stray magnetic fields.

Specifications: ASTM A753

Carpenter Technology Corporation Carpenter Technology Corporation