M-50 Bearing Steel

UNS K88165

Composition (Nominal):
0.80 C, 0.25 Mn, 0.015 P, 0.015 S, 0.25 Si, 4.00 Cr, 0.10 Ni, 4.50 Mo, 1.00 V, Bal. Fe

A premium-melted alloy exhibiting excellent resistance to multi-axial stresses and softening at high service temperatures and good resistance to oxidation.

M-50 Bearing Steel, which is refined using vacuum-induction melting (VIM) and vacuum-arc remelting (VAR) processes, exhibits excellent resistance to multi-axial stresses and softening at high service temperatures as well as good resistance to oxidation. Characteristic of a high-speed tool steel, it possesses high compressive strength.

Specifications: AISI Type M-50 | AMS 6490 | AMS 6491

PRODUCT RESOURCES

LITERATURE

Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »