Micro-Melt® BioDur® CCM® Alloy

Composition (Nominal)
0.14 C, 1.00 Mn, 1.00 Si, 26.00/30.00 Cr, 1.00 Ni, 5.00/7.00 Mo, Bal. Co, 0.25 N, 0.75 Fe

Micro-Melt BioDur CCM® alloy is a non-magnetic, cobalt-chromium-molybdenum wrought alloy exhibiting high strength, corrosion resistance, and wear resistance. This alloy is a powder metallurgy version of BioDur CCM alloy (ASTM F 1537 Alloy 1), which is a high nitrogen, low carbon wrought version of ASTM F 75 cast alloy. This alloy is equivalent to ASTM F 1537 Alloy #1.

Specifications:
ASTM F1537, ASTM F799, ISO 5832-12, ISO 5832-4

Note: While this material meets the following specifications, it may be capable of meeting or being manufactured to meet other general and customer-specific specifications.


Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »