Composition (Nominal)
1.50 C, 0.06 S, 4.75 Cr, 5.0 V, 13.0 W, 5.0 Co, Bal. Fe
A high-carbon tungsten/cobalt vanadium high-speed tool steel having excellent abrasion resistance and red hardness. The alloy is manufactured using powder metallurgy processing techniques, and hot worked into various mill forms.
Specifications: ASTM A600, QQ-T-590