Temper Tough® Alloy

UNS K63835
Composition (Nominal):
0.40 C, 0.90 Mn, 1.50 Si, 1.25 Cr, 3.80 Ni, 0.50 Mo, 0.50 Cu, 0.30 V, Bal. Fe

An arc melted, cobalt-free, high strength, high toughness quenched and tempered alloy. Attains a typical 290 ksi (1999 MPa) UTS combined with a typical range of 60-65 ksivin. (66-71 MPavm) fracture toughness.

This alloy is not a stainless alloy and may require plating or coating with a rust preventative or oil to prevent corrosion. The KIscc (as measured in a Rising Step Load Test) of Temper Tough alloy is 11.0 ksi sqrt(in.) (12.1 MPa sqrt(m)) in a 3.5% NaCl solution.