CT Vicalloy I Alloy


Single figures are nominal except where noted.
Carbon 0.03 %, Manganese 0.40 %, Silicon 0.20 %, Cobalt 52.00 %, Vanadium 10.00 %, Iron Balance

Vicalloy I is a precipitation hardened cobalt-base permanent magnet alloy. It is supplied to customers in the solution-treating condition which is very ductile. In this condition, it can be punched, formed, bent, drawn and machined.

Vicalloy I Alloy has been used for biasing magnets in meters and magnetic actuators, as magnetic coded devices, field coils for DC motors and servos, and hysteresis motor laminations.