CP Titanium Grade 2

Single figures are nominal except where noted

0.10 C, 0.03 N, 0.250 O, Bal. Ti, 0.30 Fe, 0.015 H, 0.40 Other/Total

*For ASTM B 348-99 Carbon = 0.08% maximum and ASTM
F 67-95 = 0.1% maximum. "Other, Each”= 0.1% maximum and "Other, Total" = 0.4% maximum values applicable for ASTM B 348-99 only.

Commercially pure, or CP, titanium is unalloyed. Each of the different CP grades are classified based on their level of non-titanium elements and the resultant differences in mechanical properties. Grade 2 has higher tolerable levels of iron and oxygen than Grade 1 and is widely used because it combines excellent formability and moderate strength with superior corrosion resistance. This combination of properties makes CP Grade 2 titanium a candidate for a large variety of chemical and marine as well as aerospace and medical applications.

Specifications: AMS 4902 (Sheet, Strip, Plate), AMS 4941 (Welded Tubing), AMS 4942 (Seamless Tubing), AMS 4951 (Weld Filler Metal Wire), ASTM B265 (Sheet, Strip, Plate), ASTM B348 (Bar, Billet), ASTM B367 (Castings), ASTM F67 (Unalloyed Ti for Surgical Implants), AWS A5.16-70 (Weld Filler Metal Wire and Rod)