CP Titanium Grade 4

Single figures are nominal except where noted
0.08 C, 0.05 N, 0.400 O, Bal. Ti, 0.50 Fe, 0.015 H, 0.40 Other/Total

ASTM B 348-99, "Other, Total" = 0.40% maximum and AMS 4921 rev. G = 0.3% maximum.

Commercially pure, or CP, titanium is unalloyed. Each of the different CP grades are classified based on their level of non-titanium elements and the resultant differences in mechanical properties. Grade 4 has the highest allowable oxygen and iron contents. It combines the excellent resistance to corrosion and corrosion fatigue of titanium with high strength that makes it a candidate to compete with steels and nickel alloys for many chemical and marine applications.

Specifications: AMS 4901 (Sheet, Strip, Plate), AMS 4921 (Bar, Wire, Forgings, Billet), ASTM B 381 (Forgings), ASTM B265 (Sheet, Strip, Plate), ASTM B348 (Bar, Billet), ASTM B367 (Castings), ASTM F 1341 (Wire), ASTM F 67 (Sheet, Strip, Bar), ISO 5832-2
MIL-T 9047 (Bars, Billets),