416 Project 70®+

UNS #S41600

416 Project 70®+ Stainless is an improved modification of 416, the first free-machining stainless steel, that can achieve 100 to 200% longer tool life, 15% faster machining speeds, and improved finishes. Its low frictional properties minimize scratching and galling in service, possessing better non galling properties than 410. 416 Project 70+ PDB® stainless combines the superior machinability of Project 70+ stainless with improved straightness and half-standard dimensional tolerances. This precision drawn bar has been used successfully in a variety of machining operations including CNC Swiss-type screw machines.

Type Analysis

  • Carbon (Maximum) 0.15
  • Phosphorus (Maximum) 0.06
  • Silicon (Maximum) 1
  • Manganese (Maximum) 1.2
  • Sulfur (Maximum) 0.15
  • Chromium (Nominal) 12.00 - 14.00
  • Iron (Nominal) Balance

Applications

fittings, gears, housings, lead screws, shafts, valve bodies, valve stems, and valve trim. It may be considered for parts requiring considerable machining.

Applicable Specifications

  • AMS 5610
  • ASTM A581
  • MIL-S-862
  • QQ-S-764
  • ASTM A314
  • ASTM A582
  • MIL-S-862

Bar

Flats

Hexagons

Rod

Rounds

Square

Wire