416BQ (No. 5 BQ)

UNS #S41600

416BQ (No. 5 BQ) is a balanced version of standard 416 stainless steel capable of producing a minimum hardness of Rockwell C 40 when bright hardened. The high hardness capability is obtained through very close chemistry and structure control, but it remains as machinable as 416 despite this. It can be cut rapidly and cleanly with regular metal cutting tools and can be freely ground and polished.

Type Analysis

  • Carbon (Maximum) 0.15
  • Phosphorus (Maximum) 0.06
  • Silicon (Maximum) 1
  • Manganese (Maximum) 1.25
  • Sulfur (Maximum) 0.15
  • Chromium (Nominal) 12.00-14.00
  • Iron (Nominal) Balance

Applications

cutters in food processing equipment, shafts, axles, gears, pinions, etc.

Applicable Specifications

  • AMS 5610
  • MIL-W-52263
  • ASTM A582
  • QQ-S-764

Bar

Flats

Hexagons

Rod

Rounds

Square

Wire