Conichrome®

UNS #R30008 & R30003

Conichrome® is a non-magnetic, austenitic Nickel-Cobalt-Chromium-Molybdenum alloy possessing a unique combination of extremely high strength, ductility, excellent corrosion resistance, and high fatigue strength. Manufactured using premium melting and remelting operations, the alloy has extremely good cleanliness (low inclusion content) and improved homogeniety, which are vital to the performance, properties, and functionality of this alloy in its demanding applications.

Type Analysis

  • Carbon (Maximum) 0.15
  • Phosphorus (Maximum) 0.015
  • Silicon (Maximum) 1.2
  • Nickel (Nominal) 14.0-18.0
  • Manganese (Maximum) 1.0-2.5
  • Sulfur (Maximum) 0.015
  • Chromium (Nominal) 18.5-21.5
  • Cobalt (Nominal) 39.0-42.0
  • Molybdenum (Nominal) 6.0-8.0
  • Iron (Nominal) Balance

Applications

suture wires, surgical clips, pacemaker leads, stents, vena cava filters and orthopedic nails, precision spring material in the watchmaking industry, torsion bars, seals, and performance springs for various markets.

Applicable Specifications

  • ASTM 1058
  • NACE MR0175
  • ISO5832-7
  • AMS 5833

Bar

Coil

Rod

Rounds

Strip

Wire