Keep tooth implant failure, rejection, and corrosion in check with precisely engineered materials. Carpenter Technology has set the standard for dental, orthodontic, and surgical alloys since 1889 — delivering superior quality, strength, biocompatibility, wear-resistance, and machinability to meet both doctor and patient goals.
innovating medical materials
microstructure and alloy purity
performance for superior patient outcomes
High-strength biocompatible materials resistant to corrosion and fracturing are essential for high-quality crowns, dental implants,and surgical instrumentation. Our materials have the necessary strength and low-nickel content for patients with metal sensitivities.
The addition of zirconium gives this alloy up to 50% greater tensile and fatigue strength than pure titanium, enabling smaller diameter implants
Careful additions and carbide control gives this hardenable martensitic stainless alloy superior corrosion resistance with hardness up to 51 HRC
The strongest grade of commercially pure titanium available, with excellent corrosion fatigue resistance and good ductility
Extra-low interstitial ASTM B348 Grade 23 has superior damage tolerance and better mechanical properties at cryogenic temperatures
A workhorse of the medical industry, providing the best combination of corrosion resistance, strength, and toughness of any commercially available material
Increased resistance to fatigue and distortion enables better shape retention over extended periods of time. Corrosion resistance permits longevity with regular interactions with topical fluoride based agents and oral enzymes.
Stability under high fatigue requirements and good ductility with a combination of strength and corrosion resistance
Unique combination of ultra-high tensile strength, good ductility and toughness, with excellent corrosion resistance
Carpenter Technology materials push what’s possible and improve patient lifestyles in dentistry, oral surgery, and orthodontics.
Find out how Carpenter Technology’s next-generation alloys can deliver peak performance for your dental, orthodontic, and surgical applications.