Composition (Nominal)

0.015 C, 0.50 Mn, 0.015 P, 0.010 S, 0.50 Si, 10.50/11.50 Cr, 7.50/8.50 Ni, 4.50/5.50 Mo, 8.00/9.00 Co, 1.00/1.50 Al, Bal. Fe

Custom 475® stainless is a premium-melted, high-strength martensitic precipitation-hardenable alloy that provides good corrosion resistance to atmospheric environments. This alloy is capable of the highest strength levels of any commercially available precipitation hardening stainless steel, reaching over 280 ksi without the benefit of strain hardening prior to aging.
Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.