CRS
CRS
4:00 PM EDT $23.93 +0
CRS
CRS
4:00 PM EDT $23.93 +0

Electrical Iron

Composition (Nominal)
0.02 max. C, 0.12 Mn, 0.12 Si, 0.010 P, 0.010 S, 0.20 Cr, 0.08 Ni, 0.05 V, Bal. Fe

Low-carbon iron with good direct current soft magnetic properties after heat treatment. Has been used in electro-mechanical relays, solenoids, magnetic pole and other flux-carrying components.

Specifications: ASTM A848 Alloy 1
Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.