TrimRite® Stainless

UNS S42010
Composition (Nominal)
0.15/0.30 C, 1.0 Mn, 0.04 P, 0.03 S, 1.0 Si, 13.50/15.00 Cr, 0.25/1.00 Ni, 0.40/1.00 Mo, Bal. Fe

Quench-hardenable stainless steel with hardness capability of Type 420, but with superior corrosion resistance and ductility. Has been used for self-drilling, self-tapping fasteners, cutlery, and valve shafts.

Specifications: ASTM A276, ASTM A493